Quote Originally Posted by duncan303 View Post
Hi Luciano

I have some of the SK10 I found it really sticky as if it never properly dried out, it worked well as a flux and to protect against oxidation but it just kept attracting dust.
I can remember having a hell of a time getting it off, the only product that seemed to work effectivly was Chemtronics Flux-Off.

Duncan
Hi Duncan,

After I apply the spray SK10 on the PCB, I bake the PCB for about 10 minutes in a preheated
pizza oven at about 100°C. After this treatment, the SK10 film on the PCB is dry.

Best regards,